| PROPERTIES | UNIT | TYPICAL VALUES | TEST METHOD | |
|---|---|---|---|---|
| MATT | ||||
| TREATMENT | DYNE/CM | I.S 46↑/O.S 38↑ | ||
| TENSILE STRENGTH |
MD | kg/㎟ | 8.9 | ASTM |
| TD | 13 | D-882 | ||
| ELONGATION AT BREAK |
MD | % | 158 | ASTM |
| TD | 45 | D-882 | ||
| HEAT SHRINKAGE |
MD | % | 1.2 | ASTM |
| TD | 0.1 | D-1204 | ||
| COEFFICIENT OF FRICTION |
OPP/INSIDE | US | 1.54/0.19 | ASTM |
| OPP/OPP | UK | 1.36/0.20 | D-1894 | |
| HAZE GLOSS |
BASE FILM | % | 84 | ASTM-1003 |
| 45º | 4.3 | ASTM-2457 | ||