| PROPERTIES | UNIT | TYPICAL VALUES | TEST METHOD | |
|---|---|---|---|---|
| GLOSS | ||||
| TREATMENT | DYNE/CM | I.S 46↑/O.S 38↑ | ||
| TENSILE STRENGTH |
MD | kg/㎟ | 10 | ASTM |
| TD | 14.2 | D-882 | ||
| ELONGATION AT BREAK |
MD | % | 162 | ASTM |
| TD | 42 | D-882 | ||
| HEAT SHRINKAGE |
MD | % | 1.5 | ASTM |
| TD | 0.3 | D-1204 | ||
| COEFFICIENT OF FRICTION |
OUT/INSIDE | US | 1.02/0.34 | ASTM |
| OPP/OPP | UK | 0.9/0.23 | D-1894 | |
| HAZE GLOSS |
BASE FILM | % | 1.9 | ASTM-1003 |
| 45º | 142 | ASTM-2457 | ||